Corrosion Resistant Superalloy Round Bar GH3030 Dia 15-180mm For Industrial Heating
High-Strength Hot Rolled Nickel-Chromium Alloy Rod with Exceptional Oxidation Resistance & Thermal Stability up to 800°C
- Overview
- Specifications
- Features
- Applications
- Why-Us
- FAQ
- Recommended Products
Overview of GH3030 Corrosion Resistant Superalloy Round Bar
GH3030 is an early-developed 80Ni-20Cr solid-solution strengthened high temperature superalloy round bar characterized by high thermal plasticity and outstanding oxidation resistance below 800°C. With a diameter range spanning Dia 15-180mm, this hot rolled superalloy rod maintains high chemical purity and structural stability in corrosive, high-temperature gases.
As an essential industrial heating element alloy, GH3030 exhibits excellent cold stamping workability and superior fusion welding characteristics. It is widely specified across thermal engineering, petrochemical cracking furnaces, turbine combustion liners, and heavy-duty industrial resistance heating components where consistent thermal resistance and extended service life are non-negotiable.

Technical Specifications and Chemical Purity
Our manufacturing process ensures strict adherence to ultra-high metallurgical purity, tight dimensional tolerances, and uniform microstructural grain boundaries.
Chemical Composition (Nominal % by Weight)
| Element | Carbon (C) | Chromium (Cr) | Nickel (Ni) | Titanium (Ti) | Aluminum (Al) | Iron (Fe) | Manganese (Mn) | Silicon (Si) | Phosphorus (P) | Sulfur (S) |
|---|---|---|---|---|---|---|---|---|---|---|
| Min (%) | — | 19.0 | Balance | 0.15 | — | — | — | — | — | — |
| Max (%) | 0.12 | 22.0 | Balance | 0.35 | 0.15 | 1.50 | 0.70 | 0.80 | 0.030 | 0.020 |
Physical & Mechanical Properties
| Technical Property | Value / Specification Metric |
|---|---|
| Density | 8.40 g/cm³ |
| Melting Temperature Range | 1374 - 1420 °C |
| Tensile Strength (Rm, Solution Treated) | ≥ 685 MPa |
| Yield Strength (Rp0.2) | ≥ 295 MPa |
| Elongation (A5) | ≥ 35% |
| Supply Diameter Range | Dia 15mm – Dia 180mm (Custom lengths available) |
| Delivery State | Hot Rolled, Annealed / Solution Treated, Peeled or Ground |
| Dimensional Tolerance | High-precision hot rolling and precision peeling tolerance control |
Distinctive Features
-
Superior Oxidation and Thermal Corrosion Resistance:The balanced 80Ni-20Cr metallurgical composition forms a dense, self-healing chromium oxide barrier on the bar surface, delivering outstanding resistance to high-temperature oxidation and corrosive sulfur-bearing gas atmospheres below 800°C.
-
Robust High-Temperature Plasticity and Workability: GH3030 solid-solution structure ensures high thermal plasticity during hot rolling and subsequent fabrication, enabling seamless cold forming, bending, machining, and deep-drawing without micro-cracking.
-
Exceptional Weldability and Thermal Fatigue Resistance: This hot rolled superalloy rod demonstrates outstanding welding performance under TIG, MIG, and resistance welding methods, maintaining weld joint integrity and high thermal fatigue endurance under cyclic heating operations.
-
Homogeneous Microstructure and High Creep Strength: Vacuum induction melting (VIM) paired with electroslag remelting (ESR) eliminates non-metallic inclusions and center-line segregation, ensuring reliable tensile strength and creep rupture performance in structural components.

Critical Applications for GH3030 Industrial Heating Element Alloy and Thermal Systems
-
Industrial Heating Elements & Furnace Hardware: High-temperature structural hangers, radiant tubes, heating element supports, and heat-treatment fixtures.
-
Aerospace & Gas Turbines: Combustion chamber liners, afterburner components, casing rings, and exhaust nozzles operating below 800°C.
-
Petrochemical & Chemical Processing: Pyrolysis furnace tubes, catalyst support grids, hot gas ducting, and valves exposed to cyclic thermal loads.
-
Power Generation & Metallurgical Systems: Heat exchangers, thermocouple protection sheaths, and furnace roller assemblies.

Why Partner with DLX
-
Advanced Metallurgy & Capacity: Backed by advanced VIM and ESR melting furnaces, continuous hot-rolling mills, and cold-finishing lines, our production capacity reaches 1,200 tons/month, ensuring scalable delivery and reliable lead times.
-
Full-Spectrum Quality Control: Every batch of GH3030 superalloy round bar undergoes 100% rigorous inspection, including optical emission spectrometry (OES), ultrasonic non-destructive testing (NDT), high-temperature tensile verification, and metallographic structure analysis.
-
Flexible Processing & Dimension Customization: Offering hot-rolled, centerless-ground, turned, and polished finishes across Dia 15-180mm with precision length cutting and tailored surface roughness.
-
Global B2B Engineering Support: Experienced metallurgical engineers providing comprehensive material data sheets, material test certificates (MTC 3.1), and custom machining guidance for OEM and engineering projects worldwide.


Frequently Asked Questions About GH3030 Superalloy Round Bar
Q1: What makes GH3030 ideal for industrial heating elements compared to standard stainless steels?
A1: GH3030 is a dedicated nickel-chromium solid solution superalloy that maintains high structural strength, thermal fatigue resistance, and an anti-spalling oxide layer up to 800°C, significantly outperforming conventional austenitic stainless steels in oxidation resistance and operational lifespan under continuous thermal cycling.
Q2: What surface finishes and diameter tolerances are available for Dia 15-180mm round bars?
A2: We supply hot rolled black surface, peeled/turned surface, and precision centerless-ground finishes. Diameters from 15mm to 180mm can be custom-processed with tight precision tolerance grades according to specific machining and drawing requirements.
Q3: What quality documentation is provided with every shipment?
A3: Every batch of GH3030 corrosion resistant alloy bar is accompanied by a certified Material Test Certificate (MTC 3.1) detailing chemical composition analysis, room-temperature and high-temperature mechanical properties, hardness test values, and ultrasonic non-destructive testing results.
Q4: How is the minimum order quantity (MOQ) and packaging managed for export orders?
A4: MOQ is dynamically tailored depending on the specific diameter (Dia 15-180mm), stock availability, and processing state. All round bars are securely wrapped with waterproof materials and packed into fumigated wooden crates or steel-banded bundles with anti-corrosion oil protection to ensure safe sea and air transport.